Cracks in walls: harmless or serious?

Read a crack by its shape, place and width, watch it properly and repair the cause, not just the surface.

RENOBILD engineering team · Updated 23 November 2026

Almost every house in Pakistan gets some cracks. Most are harmless and come from plaster shrinking or bricks and concrete moving differently with the heat. A few warn of a real structural problem. The shape, place and width of the crack tell you which.

Types of cracks and what they mean

CRACKUSUAL CAUSEHOW SERIOUS
Fine map-like cracks in plasterPlaster dried too fast, rich mix, no curingSurface only; fill and repaint
Straight crack where a wall meets a column or beamBrick and concrete move differently; no mesh at the jointUsually minor; repair with mesh and flexible filler
Diagonal crack from a door or window cornerStress at openings, a weak lintel or settlementWatch it; ask an engineer if it grows
Horizontal crack in a wall or below the roof slabRoof slab expanding in the heat, or soil pushing a wallNeeds an engineer’s check
Crack in a beam, column or slab, or wider than about 3 mmOverload, settlement, rusting steelSerious; get a structural survey

How to watch a crack

  1. Mark both ends of the crack with a pencil and write the date beside it.
  2. Photograph it with a ruler or coin for scale.
  3. Check again after a few weeks. A crack that grows, widens or reopens after filling is still moving.
  4. Note whether doors or windows nearby have started to jam.

How cracks are repaired

  • Find and stop the cause first: leaking pipes, bad drainage, roof heat or an overloaded slab
  • For plaster cracks, open the crack into a V, fill it and paint
  • At wall–column joints, fix mesh across the joint before replastering
  • Structural cracks need an engineer’s repair design, not just filler

Good curing and mesh at joints prevent most cracks in a new house: see our plaster and paint guide and grey structure checklist. If you plan to add a floor, read adding a floor first.

دیواروں میں دراڑیں: وجہ اور علاج

زیادہ تر دراڑیں پلستر کے سکڑنے یا اینٹ اور کنکریٹ کے الگ الگ پھیلنے سے آتی ہیں اور خطرناک نہیں ہوتیں۔ دروازے یا کھڑکی کے کونے سے ترچھی دراڑ، چھت کے نیچے افقی دراڑ، یا بیم، کالم اور سلیب میں دراڑ پر انجینئر کو دکھائیں۔ دراڑ کے دونوں سروں پر نشان لگا کر تاریخ لکھیں اور چند ہفتے بعد دیکھیں کہ بڑھ تو نہیں رہی۔ پہلے وجہ ٹھیک کریں، پھر مرمت۔

Questions people ask

Are hairline cracks in plaster dangerous?کیا پلستر میں باریک دراڑیں خطرناک ہیں؟

Usually not. Fine map-like cracks come from plaster drying too fast. Fill and repaint them.

When should I call an engineer about a crack?دراڑ پر انجینئر کو کب بلائیں؟

When a crack is in a beam, column or slab, is horizontal, is wider than about 3 mm, keeps growing or comes with jamming doors.

Why do cracks come back after filling?بھرنے کے بعد دراڑ دوبارہ کیوں آ جاتی ہے؟

The cause is still there, such as movement at a wall-column joint, roof heat, a leak or settlement. Fix the cause and use mesh where materials meet.

Need help on your own house?

Send 3–4 photos or your plot size on WhatsApp

We reply with what it probably is and the next step. Across Pakistan; overseas clients by video call.